Due to its outstanding electrical characteristics, such as the low temperature expansion coefficient, low dielectric constant and good mechanical properties, cordierite, 2MgO center dot 2Al(2)O(3)center dot 5SiO(2), is a very attractive high-temperature ceramic material. In order to accelerate the process of sintering, 2.50 mass% Bi2O3 has been added to the starting mixtures. Liquid phase sintering caused by the presence of bismuth-oxide lowers the temperature of cordierite formation. The mechanical activation of the starting mixtures (0-56 min in vibro-mill) additionally lowers sintering temperatures. The sintering process was performed at 1200, 1300, 1350 and 1400 degrees C, for 2 h. The particle size analysis (PSA) was employed in order to determine the changes in the particle size of the mechanically treated powders. The phase composition of the starting powders and sintered materials was analyzed by the X-ray diffraction method. Furthermore, scanning electron microscopy (SEM) was ...used in the analysis of the powder morphology.
Keywords:
Mechanical activation / Sintering / X-ray / SEM / CordieriteSource:
Powder Technology, 2012, 218, 157-161Publisher:
- Elsevier, Amsterdam
Funding / projects:
- Directed synthesis, structure and properties of multifunctional materials (RS-172057)
- Serbian Academy of Sciences and Arts [F-7/II]
DOI: 10.1016/j.powtec.2011.12.012
ISSN: 0032-5910
WoS: 000300526400023
Scopus: 2-s2.0-84855854130
Collections
Institution/Community
Poljoprivredni fakultetTY - JOUR AU - Obradović, N. AU - Djordjević, N. AU - Filipović, Suzana AU - Nikolić, N. AU - Kosanović, Darko AU - Mitrić, M. AU - Marković, S. AU - Pavlović, Vladimir PY - 2012 UR - http://aspace.agrif.bg.ac.rs/handle/123456789/2992 AB - Due to its outstanding electrical characteristics, such as the low temperature expansion coefficient, low dielectric constant and good mechanical properties, cordierite, 2MgO center dot 2Al(2)O(3)center dot 5SiO(2), is a very attractive high-temperature ceramic material. In order to accelerate the process of sintering, 2.50 mass% Bi2O3 has been added to the starting mixtures. Liquid phase sintering caused by the presence of bismuth-oxide lowers the temperature of cordierite formation. The mechanical activation of the starting mixtures (0-56 min in vibro-mill) additionally lowers sintering temperatures. The sintering process was performed at 1200, 1300, 1350 and 1400 degrees C, for 2 h. The particle size analysis (PSA) was employed in order to determine the changes in the particle size of the mechanically treated powders. The phase composition of the starting powders and sintered materials was analyzed by the X-ray diffraction method. Furthermore, scanning electron microscopy (SEM) was used in the analysis of the powder morphology. PB - Elsevier, Amsterdam T2 - Powder Technology T1 - Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive EP - 161 SP - 157 VL - 218 DO - 10.1016/j.powtec.2011.12.012 ER -
@article{ author = "Obradović, N. and Djordjević, N. and Filipović, Suzana and Nikolić, N. and Kosanović, Darko and Mitrić, M. and Marković, S. and Pavlović, Vladimir", year = "2012", abstract = "Due to its outstanding electrical characteristics, such as the low temperature expansion coefficient, low dielectric constant and good mechanical properties, cordierite, 2MgO center dot 2Al(2)O(3)center dot 5SiO(2), is a very attractive high-temperature ceramic material. In order to accelerate the process of sintering, 2.50 mass% Bi2O3 has been added to the starting mixtures. Liquid phase sintering caused by the presence of bismuth-oxide lowers the temperature of cordierite formation. The mechanical activation of the starting mixtures (0-56 min in vibro-mill) additionally lowers sintering temperatures. The sintering process was performed at 1200, 1300, 1350 and 1400 degrees C, for 2 h. The particle size analysis (PSA) was employed in order to determine the changes in the particle size of the mechanically treated powders. The phase composition of the starting powders and sintered materials was analyzed by the X-ray diffraction method. Furthermore, scanning electron microscopy (SEM) was used in the analysis of the powder morphology.", publisher = "Elsevier, Amsterdam", journal = "Powder Technology", title = "Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive", pages = "161-157", volume = "218", doi = "10.1016/j.powtec.2011.12.012" }
Obradović, N., Djordjević, N., Filipović, S., Nikolić, N., Kosanović, D., Mitrić, M., Marković, S.,& Pavlović, V.. (2012). Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive. in Powder Technology Elsevier, Amsterdam., 218, 157-161. https://doi.org/10.1016/j.powtec.2011.12.012
Obradović N, Djordjević N, Filipović S, Nikolić N, Kosanović D, Mitrić M, Marković S, Pavlović V. Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive. in Powder Technology. 2012;218:157-161. doi:10.1016/j.powtec.2011.12.012 .
Obradović, N., Djordjević, N., Filipović, Suzana, Nikolić, N., Kosanović, Darko, Mitrić, M., Marković, S., Pavlović, Vladimir, "Influence of mechanochemical activation on the sintering of cordierite ceramics in the presence of Bi2O3 as a functional additive" in Powder Technology, 218 (2012):157-161, https://doi.org/10.1016/j.powtec.2011.12.012 . .