dc.description.abstractMixtures of BaCO3-ZnO-TiO2 were mechanically activated using high-energy planetary ball mill during 20, 40 and 80 min. As the time of mechanical activation increased, the decrease in particle size was observed. The effect of milling on microstructure was investigated by scanning electron microscopy, as well. Sintering process was performed in air at 1100 and 1200 C for 2 h. Various phases are present within mixtures sintered at 1100 and 1200 degrees C, and almost pure BaZn2Ti4O11 phase was obtained after 80 min of milling and sintering at 1200 degrees C for 2 h.en
dc.publisherElsevier Sci Ltd, Oxford
dc.relationinfo:eu-repo/grantAgreement/MESTD/MPN2006-2010/142011/RS//
dc.relationSerbian Academy of Sciences and Arts [F-7/II]
dc.rightsrestrictedAccess
dc.sourceCeramics International
dc.subjectMillingen
dc.subjectSinteringen
dc.subjectX-ray methodsen
dc.subjectTraditional ceramicsen
dc.titleIsothermal sintering of barium-zinc-titanate ceramicsen
dc.typearticle
dc.rights.licenseARR
dc.citation.epage27
dc.citation.issue1
dc.citation.other37(1): 21-27
dc.citation.rankM21
dc.citation.spage21
dc.citation.volume37
dc.identifier.doi10.1016/j.ceramint.2010.07.001
dc.identifier.scopus2-s2.0-78649328681
dc.identifier.wos000285853500004