dc.description.abstractThe thermal,ability of aqueous polyurethanes has been measured by applying the thermogravimetric analysis, The aqueous polyurethanes (aqPUR) with catalysts of different selectivity have been studied by use of the dynamic method. To obtain degradations of 0.025, 0.05 and 0.10, employing the dynamic method, the heating rates of 0.5, 1, 2, 5 and 10 degrees C min(-1) have been used in the range of 30-500 degrees C. Using the more selective catalysts in the aqueous polyurethanes the total resulting time of the decomposition has increased at all degradation degrees and at all temperatures. This paper shows that the dynamic method based on the thermogravimetric analysis can be used to assess the thermal stability of the aqueous polyurethanes using the catalysts of different selectivity.en
dc.publisherElsevier Science Sa, Lausanne
dc.relationinfo:eu-repo/grantAgreement/MESTD/MPN2006-2010/142039/RS//
dc.rightsrestrictedAccess
dc.sourceProgress in Organic Coatings
dc.subjectaqueous polyurethanesen
dc.subjectcatalystsen
dc.subjectthermal degradationen
dc.subjectthermogravimetric analysisen
dc.titleThe thermal degradation of aqueous polyurethanes with catalysts of different selectivityen
dc.typearticle
dc.rights.licenseARR
dc.citation.epage116
dc.citation.issue2
dc.citation.other60(2): 112-116
dc.citation.rankM21
dc.citation.spage112
dc.citation.volume60
dc.identifier.doi10.1016/j.porgcoat.2007.07.004
dc.identifier.scopus2-s2.0-34948820702
dc.identifier.wos000250745100006
dc.type.versionpublishedVersion


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу