Electrical Properties of Sintered Magnesium-titanate Ceramics
(2012)
Poster presented at the conference Advanced Ceramics and Application I - Serbian Ceramic Society, Belgrade May 10-11, 2012
Influence of different pore-forming agents on wollastonite microstructures
(Belgrade : Serbian Ceramic Society, 2016)
In this study, highly porous macro- and micro-cellular wollastonite-based ceramics was synthesized. Ceramic precursor, methylhydrocyclosiloxane, together with micro-sized CaCO3, was used as starting material. After 20 min ...
Structural and electrical properties of barium-zinc-titanate ceramics sintered at 1300ºc
(Belgrade : Institute of Technical Sciences of SASA, 2010)
The aim of this work was an investigation of structural and electrical properties of sintered barium-zinc-titanate ceramics. Mixtures of BaCO3, ZnO and TiO2 were mechanically activated in a planetary ball mill up to 80 ...
Microstructure evolution and sintering kinetics of ZnO
(Belgrade : Institute of Technical Sciences of SASA, 2010)
The aim of this paper was to analyse the sintering kinetics and microstructure evolution of ZnO. Powder was isothermally sintered (15, 30, 60, 90 and 120 minutes) in the temperature range from 800 to 1200oC. The values of ...
Sintering of alumina doped with different oxides, followed by sensitive dilatometer
(Belgrade : Materials Research Society of Serbia, 2018)
Sintered alumina powder represents suitable material for usage in various industry fields (e.g., as chip carriers in electronics, microwaves, jewelry production), due to convenient physical properties, such as sinterability, ...
Reaction kinetics of mechanically activated cordierite based ceramics studied via DTA
(Ljubljana : Central and Eastern European Committee for Thermal Analysis and Calorimetry, 2015)
Cordierite, 2MgO•2Ah03•5Si02 (MAS), is a very attractive high-temperature ceramic material. In order to accelerate the process of sintering, 5.00 mass% Mo03 was added to the starting mixtures. The mechanical activation of ...
Sintering of cordierite in the presence of MoO3 and crystallization analysis
(Belgrade : Materials Research Society of Serbia, 2014)
Cordierite (MAS) is difficult to sinter because of the very narrow sintering temperature range (1300-1400ºC). Because a low temperature process is desirable, it is necessary to find functional ads which can allow easier ...
Shungite - a Russian mineral: possible application as a microwave absorber
(Belgrade : Materials Research Society of Serbia, 2018)
The paper presents results of investigation of the influence of mechanical activation of shungite, a Russian natural mineral rich in silica and carbon, on its sintering behavior. The mechanical activation of the starting ...