The effect of Hot Isostatic Pressing on the MT sample densities
(Belgrade : Serbian Ceramic Society, 2015)
Mechanically activated powders (0, 10, 40, 80 and 160 minutes) were formed by isostatic pressure 300 MPa to cylindrical green bodies (φ 12 mm). First set of samples was sintered at 1300°C for 30 min in air (heating rate ...
Structural characterization of mechanically activated MgO-TiO2 system
(Belgrade : Serbian Ceramic Society, 2013)
In this article the influence of ball miling process on structure of MgO-TiO2 system was investigated. The mixtures of MgO-TiO2 powders were mechanically activated in a planetary ball mill for the time period from 0 to 120 ...