Grain growth during sintering of batio3 with lif

Pavlović, Vladimir; Stojanović, Biljana D.; Zivković, Ljiljana; Branković, Goran; Ristić, Momčilo M.

(Taylor & Francis Ltd, Abingdon, 1996)

TY  - JOUR
AU  - Pavlović, Vladimir
AU  - Stojanović, Biljana D.
AU  - Zivković, Ljiljana
AU  - Branković, Goran
AU  - Ristić, Momčilo M.
PY  - 1996
UR  - http://aspace.agrif.bg.ac.rs/handle/123456789/101
AB  - The sintering behavior of BaTiO3 with LiF showed that it was possible to sinter barium titanate at temperatures below 1000 degrees C. Different combinations of the sintering powders were prepared by adding 1 to 5 w% LiF and sintering at the temperature of 950 degrees C for 20 hours. The grain growth of LiF fluxed BaTiO3 was studied, and electron microscopy was used to investigate and characterize the microstructure of the samples. The dielectric constant and dielectric losses were determined. It was shown that the composition of the liquid phase formed during this process had a prominent influence on the grain growth and on the formation of BaTiO3 with better dielectric properties.
PB  - Taylor & Francis Ltd, Abingdon
T2  - Ferroelectrics
T1  - Grain growth during sintering of batio3 with lif
EP  - 168
SP  - 165
VL  - 186
DO  - 10.1080/00150199608218057
ER  - 
@article{
author = "Pavlović, Vladimir and Stojanović, Biljana D. and Zivković, Ljiljana and Branković, Goran and Ristić, Momčilo M.",
year = "1996",
abstract = "The sintering behavior of BaTiO3 with LiF showed that it was possible to sinter barium titanate at temperatures below 1000 degrees C. Different combinations of the sintering powders were prepared by adding 1 to 5 w% LiF and sintering at the temperature of 950 degrees C for 20 hours. The grain growth of LiF fluxed BaTiO3 was studied, and electron microscopy was used to investigate and characterize the microstructure of the samples. The dielectric constant and dielectric losses were determined. It was shown that the composition of the liquid phase formed during this process had a prominent influence on the grain growth and on the formation of BaTiO3 with better dielectric properties.",
publisher = "Taylor & Francis Ltd, Abingdon",
journal = "Ferroelectrics",
title = "Grain growth during sintering of batio3 with lif",
pages = "168-165",
volume = "186",
doi = "10.1080/00150199608218057"
}
Pavlović, V., Stojanović, B. D., Zivković, L., Branković, G.,& Ristić, M. M.. (1996). Grain growth during sintering of batio3 with lif. in Ferroelectrics
Taylor & Francis Ltd, Abingdon., 186, 165-168.
https://doi.org/10.1080/00150199608218057
Pavlović V, Stojanović BD, Zivković L, Branković G, Ristić MM. Grain growth during sintering of batio3 with lif. in Ferroelectrics. 1996;186:165-168.
doi:10.1080/00150199608218057 .
Pavlović, Vladimir, Stojanović, Biljana D., Zivković, Ljiljana, Branković, Goran, Ristić, Momčilo M., "Grain growth during sintering of batio3 with lif" in Ferroelectrics, 186 (1996):165-168,
https://doi.org/10.1080/00150199608218057 . .
6
7
6