Barium-Strontium-Titanate Ba0.77Sr0.23TiO3 was prepared from starting materials BaCO3, SrCO3 and TiO2 through solid-state reactions. Mixtures of these oxides are mechanically activated in a high-energy planetary ball mill at different time intervals from 0 to 120 minutes. In order to obtain information on phase composition, crystal structure was determent by X-ray diffraction. It was observed that after 80 minutes in process synthesis Ba0.77Sr0.23TiO3 started Thermal analyzes were performed in order to determine the characteristic temperatures of the processes that occur in the solid phase. Particle size distribution, together with electron microscopy scanning has given us very useful information about the morphology of the powder.
Кључне речи:
Mechanical activation / Scanning electron microscopy / Crystal structure / Barium-strontium-titanateИзвор:
Science of Sintering, 2012, 44, 1, 47-55Издавач:
- Međunarodni Institut za nauku o sinterovanju, Beograd
Финансирање / пројекти:
- Усмерена синтеза, структура и својства мултифункционалних материјала (RS-MESTD-Basic Research (BR or ON)-172057)
- Serbian Academy of Sciences and Arts [F-198]
- NSF CRESTNational Science Foundation (NSF)NSF- Directorate for Education & Human Resources (EHR) [HRD-0833184]
- NASANational Aeronautics & Space Administration (NASA) [NNX09AV07A]
- Direct For Education and Human ResourcesNational Science Foundation (NSF)NSF- Directorate for Education & Human Resources (EHR) [0833184] Funding Source: National Science Foundation
- Division Of Human Resource DevelopmentNational Science Foundation (NSF)NSF- Directorate for Education & Human Resources (EHR) [0833184] Funding Source: National Science Foundation
DOI: 10.2298/SOS1201047K
ISSN: 0350-820X
WoS: 000318147700005
Scopus: 2-s2.0-84864299572
Институција/група
Poljoprivredni fakultetTY - JOUR AU - Kosanović, Darko AU - Obradović, N. AU - Zivojinović, J. AU - Filipović, Suzana AU - Maricić, A. AU - Pavlović, Vladimir AU - Tang, Y. AU - Ristić, M.M. PY - 2012 UR - http://aspace.agrif.bg.ac.rs/handle/123456789/3040 AB - Barium-Strontium-Titanate Ba0.77Sr0.23TiO3 was prepared from starting materials BaCO3, SrCO3 and TiO2 through solid-state reactions. Mixtures of these oxides are mechanically activated in a high-energy planetary ball mill at different time intervals from 0 to 120 minutes. In order to obtain information on phase composition, crystal structure was determent by X-ray diffraction. It was observed that after 80 minutes in process synthesis Ba0.77Sr0.23TiO3 started Thermal analyzes were performed in order to determine the characteristic temperatures of the processes that occur in the solid phase. Particle size distribution, together with electron microscopy scanning has given us very useful information about the morphology of the powder. PB - Međunarodni Institut za nauku o sinterovanju, Beograd T2 - Science of Sintering T1 - Mechanical-Chemical Synthesis Ba0.77Sr0.23TiO3 EP - 55 IS - 1 SP - 47 VL - 44 DO - 10.2298/SOS1201047K ER -
@article{ author = "Kosanović, Darko and Obradović, N. and Zivojinović, J. and Filipović, Suzana and Maricić, A. and Pavlović, Vladimir and Tang, Y. and Ristić, M.M.", year = "2012", abstract = "Barium-Strontium-Titanate Ba0.77Sr0.23TiO3 was prepared from starting materials BaCO3, SrCO3 and TiO2 through solid-state reactions. Mixtures of these oxides are mechanically activated in a high-energy planetary ball mill at different time intervals from 0 to 120 minutes. In order to obtain information on phase composition, crystal structure was determent by X-ray diffraction. It was observed that after 80 minutes in process synthesis Ba0.77Sr0.23TiO3 started Thermal analyzes were performed in order to determine the characteristic temperatures of the processes that occur in the solid phase. Particle size distribution, together with electron microscopy scanning has given us very useful information about the morphology of the powder.", publisher = "Međunarodni Institut za nauku o sinterovanju, Beograd", journal = "Science of Sintering", title = "Mechanical-Chemical Synthesis Ba0.77Sr0.23TiO3", pages = "55-47", number = "1", volume = "44", doi = "10.2298/SOS1201047K" }
Kosanović, D., Obradović, N., Zivojinović, J., Filipović, S., Maricić, A., Pavlović, V., Tang, Y.,& Ristić, M.M.. (2012). Mechanical-Chemical Synthesis Ba0.77Sr0.23TiO3. in Science of Sintering Međunarodni Institut za nauku o sinterovanju, Beograd., 44(1), 47-55. https://doi.org/10.2298/SOS1201047K
Kosanović D, Obradović N, Zivojinović J, Filipović S, Maricić A, Pavlović V, Tang Y, Ristić M. Mechanical-Chemical Synthesis Ba0.77Sr0.23TiO3. in Science of Sintering. 2012;44(1):47-55. doi:10.2298/SOS1201047K .
Kosanović, Darko, Obradović, N., Zivojinović, J., Filipović, Suzana, Maricić, A., Pavlović, Vladimir, Tang, Y., Ristić, M.M., "Mechanical-Chemical Synthesis Ba0.77Sr0.23TiO3" in Science of Sintering, 44, no. 1 (2012):47-55, https://doi.org/10.2298/SOS1201047K . .