Sintering of Mechanically Activated Magnesium-titanate and Barium-zinc-titanate Ceramics
2011
Аутори
Obradović, N.Filipović, Suzana
Pavlović, Vladimir
Maricić, A.
Mitrović, N.
Balac, I.
Ristić, M.M.
Чланак у часопису (Објављена верзија)
Метаподаци
Приказ свих података о документуАпстракт
In this article the influence of mechanical activation on sintering process of magnesium-titanate and barium-zinc-titanate ceramics has been investigated. Both non-activated and mixtures treated in planetary ball mill for 80 minutes were sintered at 1100 degrees C and 1300 degrees C. The influence of mechanical activation on phase composition and crystal structure has been analyzed by XRD, while the effect of activation and sintering process on microstructure was investigated by scanning electron microscopy. It has been established that temperature of 1100 degrees C was to low to induce final sintering stage for both systems. Moreover, we concluded that barium-zinc-titanate ceramics exhibited better sinterability than magnesium-titanate ceramics.
Кључне речи:
Ceramics / Mechanochemical processing / Sintering / SEMИзвор:
Science of Sintering, 2011, 43, 2, 145-151Издавач:
- Međunarodni Institut za nauku o sinterovanju, Beograd
Финансирање / пројекти:
- Serbian Academy of Sciences and Arts
- Усмерена синтеза, структура и својства мултифункционалних материјала (RS-172057)
- Синтеза, развој технологија добијања и примена наноструктурних мултифункционалних материјала дефинисаних својстава (RS-45019)
DOI: 10.2298/SOS1102145O
ISSN: 0350-820X
WoS: 000296942600004
Scopus: 2-s2.0-80054101317
Институција/група
Poljoprivredni fakultetTY - JOUR AU - Obradović, N. AU - Filipović, Suzana AU - Pavlović, Vladimir AU - Maricić, A. AU - Mitrović, N. AU - Balac, I. AU - Ristić, M.M. PY - 2011 UR - http://aspace.agrif.bg.ac.rs/handle/123456789/2676 AB - In this article the influence of mechanical activation on sintering process of magnesium-titanate and barium-zinc-titanate ceramics has been investigated. Both non-activated and mixtures treated in planetary ball mill for 80 minutes were sintered at 1100 degrees C and 1300 degrees C. The influence of mechanical activation on phase composition and crystal structure has been analyzed by XRD, while the effect of activation and sintering process on microstructure was investigated by scanning electron microscopy. It has been established that temperature of 1100 degrees C was to low to induce final sintering stage for both systems. Moreover, we concluded that barium-zinc-titanate ceramics exhibited better sinterability than magnesium-titanate ceramics. PB - Međunarodni Institut za nauku o sinterovanju, Beograd T2 - Science of Sintering T1 - Sintering of Mechanically Activated Magnesium-titanate and Barium-zinc-titanate Ceramics EP - 151 IS - 2 SP - 145 VL - 43 DO - 10.2298/SOS1102145O ER -
@article{ author = "Obradović, N. and Filipović, Suzana and Pavlović, Vladimir and Maricić, A. and Mitrović, N. and Balac, I. and Ristić, M.M.", year = "2011", abstract = "In this article the influence of mechanical activation on sintering process of magnesium-titanate and barium-zinc-titanate ceramics has been investigated. Both non-activated and mixtures treated in planetary ball mill for 80 minutes were sintered at 1100 degrees C and 1300 degrees C. The influence of mechanical activation on phase composition and crystal structure has been analyzed by XRD, while the effect of activation and sintering process on microstructure was investigated by scanning electron microscopy. It has been established that temperature of 1100 degrees C was to low to induce final sintering stage for both systems. Moreover, we concluded that barium-zinc-titanate ceramics exhibited better sinterability than magnesium-titanate ceramics.", publisher = "Međunarodni Institut za nauku o sinterovanju, Beograd", journal = "Science of Sintering", title = "Sintering of Mechanically Activated Magnesium-titanate and Barium-zinc-titanate Ceramics", pages = "151-145", number = "2", volume = "43", doi = "10.2298/SOS1102145O" }
Obradović, N., Filipović, S., Pavlović, V., Maricić, A., Mitrović, N., Balac, I.,& Ristić, M.M.. (2011). Sintering of Mechanically Activated Magnesium-titanate and Barium-zinc-titanate Ceramics. in Science of Sintering Međunarodni Institut za nauku o sinterovanju, Beograd., 43(2), 145-151. https://doi.org/10.2298/SOS1102145O
Obradović N, Filipović S, Pavlović V, Maricić A, Mitrović N, Balac I, Ristić M. Sintering of Mechanically Activated Magnesium-titanate and Barium-zinc-titanate Ceramics. in Science of Sintering. 2011;43(2):145-151. doi:10.2298/SOS1102145O .
Obradović, N., Filipović, Suzana, Pavlović, Vladimir, Maricić, A., Mitrović, N., Balac, I., Ristić, M.M., "Sintering of Mechanically Activated Magnesium-titanate and Barium-zinc-titanate Ceramics" in Science of Sintering, 43, no. 2 (2011):145-151, https://doi.org/10.2298/SOS1102145O . .